Zeitschriftenartikel (3603)
3341.
Zeitschriftenartikel
151, 7, S. B446 - B452 (2004)
Semiconsucting behavior of temporarily protective oil coating on the surface of AISI 304 satinles steel in 5% Na2SO4 soultion during its degradation. Journal of the Electrochemical Society 3342.
Zeitschriftenartikel
151 (7), S. B446 - B452 (2004)
Semiconducting behavior of temporarily protective oil coating on the surface of AISI 304 stainless steel in 5% Na2SO4 solution during its degradation. Journal of the Electrochemical Society 3343.
Zeitschriftenartikel
54, S. 860 - 893 (2003)
Metal Dusting Resistance of High Chromium-Alloys. Material and Corrosion 3344.
Zeitschriftenartikel
54 (10), S. 799 - 804 (2003)
Occurrence of Metal Dusting - Referring to Failure Cases. Material and Corrosion 3345.
Zeitschriftenartikel
54, S. 785 - 792 (2003)
Metal Dusting Behaviour of Welded Ni-Base Alloys with Different Surface Finish. Material and Corrosion 3346.
Zeitschriftenartikel
54 (10), S. 778 - 784 (2003)
Metal dusting of ferritic Fe–Al–M–C (M=Ti, V, Nb, Ta) alloys in CO–H2–H2O gas mixtures at 650 °C. Materials and Corrosion 3347.
Zeitschriftenartikel
A 353 (1-2), S. 80 - 86 (2003)
APFIM investigations on quasi-binary hypoeutectic NiAl–Re alloys. Materials Science and Engineering A: Structural Materials Properties Microstructure and Processing 3348.
Zeitschriftenartikel
74 (7), S. 453 - 458 (2003)
Delamination resistant zinc alloys: Simple concept and results on the system zinc-magnesium. Steel Research International 3349.
Zeitschriftenartikel
150 (6), S. A835 - A849 (2003)
Mechanism of atmospheric corrosion of copper in the presence of ammonium sulphate particles - Effect of surface particle concentration. Journal of the Electrochemical Society 3350.
Zeitschriftenartikel
136 (1-3), S. 114 - 119 (2003)
Production scale processing of a new intermetallic NiAl-Ta-Cr alloy for high-temperature application: Part II. Powder metallurgical production of bolts by hot isostatic pressing. Journal of Materials Processing Technology 3351.
Zeitschriftenartikel
136 (1-3), S. 105 - 113 (2003)
Production-scale processing of a new intermetallic NiAl-Ta-Cr alloy for high-temperature application: Part I. Production of master alloy remelt ingots and investment casting of combustor liner model panels. Journal of Materials Processing Technology 3352.
Zeitschriftenartikel
11 (5), S. 443 - 450 (2003)
Constitution and microstructures of Fe–Al–M–C (M=Ti, V, Nb, Ta) alloys with carbides and Laves phase. Intermetallics 3353.
Zeitschriftenartikel
48, 9, S. 1093 - 1324 (2003)
Microscopic and nanoscopic aspects of corrosion and corrosion protection. Electrochimica Acta 3354.
Zeitschriftenartikel
48 (9), S. 1235 - 1243 (2003)
Microscopic aspects of electrochemical delamination: An SKPFM study. Electrochimica Acta 3355.
Zeitschriftenartikel
48 (9), S. 1211 - 1222 (2003)
The Role of Chromate in Filiform Corrosion Inhibition. Electrochimica Acta 3356.
Zeitschriftenartikel
94 (4), S. 396 - 410 (2003)
A Re-examination of the Liquidus Surface of the Al–Fe–Ti System. Zeitschrift für Metallkunde 3357.
Zeitschriftenartikel
45 (2), S. 281 - 299 (2003)
Effect of Gas Composition on Cementite Decomposition and Coke Formation of Iron. Corrosion Science 3358.
Zeitschriftenartikel
54 (2), S. 97 - 105 (2003)
Study of electronic-ionic conducting transformation of temporarily protective oil coating in salt solution. Materials and Corrosion-Werkstoffe und Korrosion 3359.
Zeitschriftenartikel
173-174, S. 996 - 1001 (2003)
Tailored thin plasma polymers for the corrosion protection of metals. Surface and Coatings Technology 3360.
Zeitschriftenartikel
51, S. 1755 - 1765 (2003)
Effects of Topology on Abnormal Grain Growth in Silicon Steel. Acta Materialia